Topic 04 · Fluid Lines and Fittings
Set C Questions 21 to 28
- 21
Which fitting standard is identified by a blue anodised finish?
Explanation
Blue anodising marks aluminium AN fittings. Steel AN fittings are cadmium plated and look silver or grey.
- 22
What must be checked before making up a flared tube joint?
Explanation
A flare with a score line in it will leak at pressure no matter how tight the nut is.
- 23
What is the purpose of the sleeve in a flared tube connection?
Explanation
Without the sleeve the nut would drag on the flare face and tear it as the joint is tightened.
- 24
What is a flareless fitting sealed by?
Explanation
The ferrule is preset first, then the joint is made up to a specified number of turns rather than to feel.
- 25
What should be done with a fluid line that has a dent in a bend?
Explanation
Dents in a straight portion may be acceptable within limits. A dent in a bend is a rejection.
- 26
Why must fluid lines be supported at regular intervals along a run?
Explanation
The failure shows up at the fitting because that is where the vibration is restrained and the stress concentrates.
- 27
What is the danger of a chafing fluid line?
Explanation
A chafed fuel or hydraulic line is a fire or a system loss. Clamping and separation from structure is what prevents it.
- 28
What must never be used to clean the inside of a fluid line?
Explanation
Residue and lint travel downstream and jam valves. Blow lines out and cap them until they are installed.